A tube, dried by fanning with a flame and prepared for evacuation
and melt-sealing, is charged with a small amount of Nbl5 under
completely anhydrous conditions. The tube is then sealed in a high vacuum and the end containing
Nbl5 is heated to 270°Cwhile the reactor is in a horizontal position.
The liberated iodine collects at the other end, which is kept at a
temperature of about 35°C (p[I2] = 0.8 mm.). The reaction time is
about 48 hours. A residue of Nbl4 remains on the spot where the
starting Nbl5
was placed; it can be sublimed at about 300 °C under
the above-indicated I2 pressure. Nbl5= Nbl4 + 1/2
I2.